Trigonox K80 Resin avec agent de durcissement à température ambiante
$3.61-19 Others
$3.5820-999 Others
$3.5≥1000Others
Type de paiement: | L/C,Western Union,T/T |
Hafen: | Shanghai Port of China |
$3.61-19 Others
$3.5820-999 Others
$3.5≥1000Others
Type de paiement: | L/C,Western Union,T/T |
Hafen: | Shanghai Port of China |
Modèle: Trigonox K80
marque: Nouryon
Classification: Agent auxiliaire chimique
CAS No.: 80-15-9
Other Names: CHP, cumene hydroperoxide
MF: C3h5no)n
EINECS No.: 201-254-7
Type: plastic curing agent
Usage: Plastic Auxiliary Agents
Brand Name: Trigonox
Model Number: Trigonox K-90
Nom du produit: cumene hydroperoxide
Appearance: Clear Liquid
Description du produit: CHP
Certification: Msds
Function: catalyst
Détails d'emballage: 20kg/barrel
Packaging Materlal: plastic barrel
Assay: 87.0-90.0%
Density: 1.06 g/cm3
Purity: 100%
Place Of Origin: Jiangsu, China
Model: Trigonox K-90
Lieu D'origine: Chine
Unités de vente | : | kilogram |
Type de colis | : | baril en plastique |
Exemple d’image | : |
The file is encrypted. Please fill in the following information to continue accessing it
Trigonox K80 Nouryon CHP Cumene Hydroperoxyde CAS 80159
Trigonox K-90 peut être utilisé comme agent de durcissement pour le polyester insaturé Résines.
Sans l'ajout d'un accélérateur, la polymérisation ne commence qu'au-dessus de la température d'activation de 90 ° C. Pour la guérison à des températures à basse température K-90 , doit être accélérée par le cobalt ou le vanadium. Ensemble avec Accélérateurs de cobalt Le temps de gel à température ambiante est très long et est donc particulièrement adapté aux applications où un long temps de production est requis, par exemple dans la production de grandes pièces et dans l'enroulement du filament. Des temps de gel et de guérison suffisamment rapides ne sont obtenus que supérieurs à 35 ° C.
Avec les accélérateurs de vanadium, le trigonox K-90 donne un temps de gel court et un remède rapide à température ambiante. Cela peut être amélioré davantage en ajoutant un promoteur spécial, comme l'acide pyruvique. Avec un tel système, il est possible d'obtenir un remède rapide de résines UP, même à basse température. Également pour les résines comme la résine vinylester, ces combinaisons sont très appropriées.
Product description |
Cumyl hydroperoxide, 90% in aromatic solvent mixture |
|||||||||||||
|
|
|
|
|
|
|
|
|
CH3 |
|
|
|||
|
|
|
|
|
|
|
|
|
|
|||||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
C |
|
O |
|
OH |
|
||
|
|
|
|
|
|
|
|
|
|
|||||
|
|
|
|
|
|
|
|
|
CH3 |
|
|
|||
|
|
|
|
|
|
|
|
|
|
|||||
|
Molecular weight |
|
: 152.2 |
|||||||||||
|
Active oxygen content peroxide |
: 10.51% |
||||||||||||
|
CAS No. |
|
: 80-15-9 |
|||||||||||
|
EINECS/ELINCS No. |
|
: 201-254-7 |
|||||||||||
|
TSCA status |
|
: listed on inventory |
|||||||||||
Specifications |
Appearance |
|
: Clear liquid |
|||||||||||
|
Assay |
|
: 87.0-90.0% |
|||||||||||
|
Color |
|
: 200 Pt-Co max. |
|||||||||||
|
Active Oxygen |
|
: 9.14-9.46% |
|||||||||||
Characteristics |
Density, 20°C |
|
: 1.06 g/cm3 |
|||||||||||
|
Viscosity, 20°C |
|
: 10.9 mPa.s |
|||||||||||
Storage |
Due to the relatively unstable nature of organic peroxides a loss of quality |
|||||||||||||
|
can be detected over a period of time. To minimize the loss of quality, |
|||||||||||||
|
AkzoNobel recommends a maximum storage temperature (Ts max.) for |
|||||||||||||
|
each organic peroxide product. |
|
||||||||||||
|
For Trigonox K-90 |
Ts max. = 40°C and |
||||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
|
Ts min. = -30°C to prevent crystallization |
|
|
When stored under these recommended storage conditions, Trigonox K-90 |
|||||||||||||
|
will remain within the AkzoNobel specifications for a period of at least 3 |
|||||||||||||
|
months after delivery. |
|
|
|||||||||||
Thermal stability |
Organic peroxides are thermally unstable substances, which may undergo |
|||||||||||||
|
self-accelerating decomposition. The lowest temperature at which self- |
|||||||||||||
|
accelerating decomposition of a substance in the original packaging may |
|||||||||||||
|
occur is the Self-Accelerating Decomposition Temperature (SADT). The |
|||||||||||||
|
SADT is determined on the basis of the Heat Accumulation Storage Test. |
|||||||||||||
|
For Trigonox K-90 |
SADT : 70°C |
|
|||||||||||
|
The Heat Accumulation Storage Test is a recognized test method for the determination of the |
|||||||||||||
|
SADT of organic peroxides (see Recommendations on the Transport of Dangerous Goods, |
|||||||||||||
|
Manual of Tests and Criteria - United Nations, New York and Geneva). |
|||||||||||||
Major decomposition |
Acetophenone, 2-Phenylisopropanol, Methane |
|||||||||||||
products |
|
|
|
|
|
|
|
|
|
|
|
|
|
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.